Material Characteristics | |||||||
Material Properties | Symbol | Unit | Measuring Conditions | SFP300T | |||
Freq. | Flux den. | Temp. | |||||
Initial Permeability | μi | ≤10kHz | 0.25mT | 25°C | 300±20% | ||
Power Loss | Pv | kW/m3 | 25kHz | 200mT | 25 °C | ||
100°C | |||||||
100kHz | 200mT | 25 °C | |||||
100°C | |||||||
300kHz | 100mT | 25 °C | |||||
100°C | |||||||
500kHz | 50mT | 25 °C | |||||
100°C | |||||||
Saturation Flux Density | Bms | mT | 10KHz | H=1200A/m | 25°C | 4000 | |
100°C | |||||||
Remanence | Brms | mT | 10KHz | H=1200A/m | 25°C | ≥2400 | |
100°C | |||||||
Coercivity | Hc | A/m | 10kHz | H=1200A/m | 25°C | 0.3 | |
100°C | |||||||
Relative Loss Factor | tanδ /µi | 10-6 | 10KHz | <0.25mT | 25°C | ||
100kHz | 25°C | ||||||
Hysteresis Material Constant | ηB | 10-6/mT | 10KHz | 1.5-3.0mT | 25°C | ||
Disaccommodation Factor | DF | 10-6 | 10KHz | < 0.25mT | 25°C | ||
Curie Temperature | Tc | °C | ≥180 | ||||
Resistivity | ρ | Ωm | ≥1000 | ||||
Density | d | g/cm3 | 4.9 | ||||